Bayan an ƙera alloy ɗin aluminium zuwa ingot na aluminum, yana wucewa ta matakai uku don zama radiator:
1. The extruder sanya ingot cikin aluminum extruded mashaya, sarrafa kamar yadda a kasa:
a.Ana ciyar da ingot na aluminium a cikin injin ƙirar aluminium, mai zafi zuwa 500 ° C kuma an tura shi ta hanyar extrusion na aluminium (kuma mai zafi zuwa 380 ° C don guje wa gurɓataccen ƙura).
b.Tempo ko tsufa magani, ƙara taurin don sauƙi na gaba yanke & sarrafawa;Maganin tsufa yana buƙatar gasa a 185 ° C na tsawon awanni 6 (awanni 3.5 a 190 ° C, awanni 2 da mintuna 20 a 200 ° C).
c.Sanyaya, yankan (mita 5 ~ 6 a kowace naúrar), dubawa, marufi da ajiya ko jigilar kaya.
2. Aluminum extruded tsiri da ake sarrafa a cikin zafi nutse
3. Mai sarrafa zafi da fan… Da sauransu, an haɗa su cikin na'urar radiyo